Publikationen

AG Thermo-iono-elektronische Materialien und Mikrostrukturanalytik

2013


Ravkina, O., Klande, T., & Feldhoff, A. (2013). Investigation of Zr-doped BSCF perovskite membrane for oxygen separation in the intermediate temperature range. Journal of solid state chemistry, 201, 101-106. https://doi.org/10.1016/j.jssc.2013.02.023
Wei, Y., Ravkina, O., Klande, T., Wang, H., & Feldhoff, A. (2013). Effect of CO2 and SO2 on oxygen permeation and microstructure of (Pr0.9La0.1)2(Ni0.74Cu0.21Ga0.05)O4+δ membranes. Journal of membrane science, 429, 147-154. https://doi.org/10.1016/j.memsci.2012.11.075
Wulf, E., Alphei, L. D., Westphal, D., Seitz, J.-M., Schaper, M., Becker, J. A., Feldhoff, A., & Bach, F.-W. (2013). Grain refining of aluminium alloys and silicon by means of boron-nitride particles. International Journal of Materials Research. https://doi.org/10.3139/146.110866
Zhou, W., Sunarso, J., Zhao, M., Liang, F., Klande, T., & Feldhoff, A. (2013). A highly active perovskite electrode for the oxygen reduction reaction below 600 °c. Angewandte Chemie - International Edition, 52(52), 14036-14040. https://doi.org/10.1002/anie.201307305

2012


Efimov, K., Klande, T., Juditzki, N., & Feldhoff, A. (2012). Ca-containing CO2-tolerant perovskite materials for oxygen separation. Journal of membrane science, 389, 205-215. https://doi.org/10.1016/j.memsci.2011.10.030
Klande, T., Cusenza, S., Gaczyński, P., Becker, K. D., Dörrer, L., Borchardt, G., & Feldhoff, A. (2012). In-situ Mössbauer studies of 57Fe-doped Ruddlesden-Popper type lanthanum nickel oxides. Solid State Ionics, 222-223, 8-15. https://doi.org/10.1016/j.ssi.2012.06.019
Robben, L., Ismail, A. A., Lohmeier, S. J., Feldhoff, A., Bahnemann, D. W., & Buhl, J.-C. (2012). Facile Synthesis of Highly Ordered Mesoporous and Well Crystalline TiO2: Impact of Different Gas Atmosphere and Calcination Temperatures on Structural Properties. Chemistry of materials, 24(7), 1268–1275. https://doi.org/10.1021/cm203203b
Senna, M., Šepelák, V., Shi, J., Bauer, B., Feldhoff, A., Laporte, V., & Becker, K. D. (2012). Introduction of oxygen vacancies and fluorine into TiO 2 nanoparticles by co-milling with PTFE. Journal of solid state chemistry, 187, 51-57. https://doi.org/10.1016/j.jssc.2011.12.036
Šepelák, V., Myndyk, M., Fabián, M., Da Silva, K. L., Feldhoff, A., Menzel, D., Ghafari, M., Hahn, H., Heitjans, P., & Becker, K. D. (2012). Mechanosynthesis of nanocrystalline fayalite, Fe2SiO4. Chemical communications, 48(90), 11121-11123. https://doi.org/10.1039/c2cc36370d
Šepelák, V., Becker, S. M., Bergmann, I., Indris, S., Scheuermann, M., Feldhoff, A., Kübel, C., Bruns, M., Stürzl, N., Ulrich, A. S., Ghafari, M., Hahn, H., Grey, C. P., Becker, K. D., & Heitjans, P. (2012). Nonequilibrium structure of Zn2SnO 4 spinel nanoparticles. Journal of Materials Chemistry, 22(7), 3117-3126. https://doi.org/10.1039/c2jm15427g