Publikationen

AG Thermo-iono-elektronische Materialien und Mikrostrukturanalytik

2022


Wolf, M., Flormann, J., Steinhoff, T., Gerstein, G., Nürnberger, F., Maier, H. J., & Feldhoff, A. (2022). Cu-Ni-Based Alloys from Nanopowders as Potent Thermoelectric Materials for High-Power Output Applications. Alloys, 1(1), 3-14. https://doi.org/10.3390/alloys1010002, https://doi.org/10.15488/12229
Zhao, Z., Rehder, L., Steinbach, F., & Feldhoff, A. (2022). High-Entropy Perovskites Pr1−xSrx(Cr,Mn,Fe,Co,Ni)O3−δ (x = 0–0.5): Synthesis and Oxygen Permeation Properties. Membranes, 12(11), Artikel 1123. https://doi.org/10.3390/membranes12111123
Zhao, Z., Ding, L., Hinterding, R., Mundstock, A., Belke, C., Haug, R. J., Wang, H., & Feldhoff, A. (2022). MXene assisted preparation of well-intergrown ZIF-67 membrane for helium separation. Journal of membrane science, 652, Artikel 120432. https://doi.org/10.1016/j.memsci.2022.120432

2021


Alahmad, A., Feldhoff, A., Bigall, N. C., Rusch, P., Scheper, T., & Walter, J. G. (2021). Hypericum perforatum L.-mediated green synthesis of silver nanoparticles exhibiting antioxidant and anticancer activities. Nanomaterials, 11(2), 1-26. Artikel 487. https://doi.org/10.3390/nano11020487
Buck, F., Feldhoff, A., Caro, J., & Schiestel, T. (2021). Permeation improvement of LCCF hollow fiber membranes by spinning and sintering optimization. Separation and Purification Technology, 259, Artikel 118023. https://doi.org/10.1016/j.seppur.2020.118023
Chen, G., Zhao, Z., Widenmeyer, M., Frömling, T., Hellmann, T., Yan, R., Qu, F., Homm, G., Hofmann, J. P., Feldhoff, A., & Weidenkaff, A. (2021). A comprehensive comparative study of CO2-resistance and oxygen permeability of 60 wt % Ce0.8M0.2O2–δ (M = La, Pr, Nd, Sm, Gd) - 40 wt % La0.5Sr0.5Fe0.8Cu0.2O3–δ dual-phase membranes. Journal of membrane science, 639, Artikel 119783. https://doi.org/10.1016/j.memsci.2021.119783
Hinterding, R., Zhao, Z., Wolf, M., Jakob, M., Oeckler, O., & Feldhoff, A. (2021). Ceramic composites based on Ca3Co4−xO9+δ and La2NiO4+δ with enhanced thermoelectric properties. Open Ceramics, 6, Artikel 100103. https://doi.org/10.1016/j.oceram.2021.100103
Hinterding, R., Wolf, M., Jakob, M., Oeckler, O., & Feldhoff, A. (2021). Improved thermoelectric properties in ceramic composites based on Ca3Co4O9 and Na2Ca2Nb4O13. Open Ceramics, 8, Artikel 100198. https://doi.org/10.1016/j.oceram.2021.100198
Kißling, P. A., Lübkemann, F., von Bronk, T., Cotardo, D., Lei, L., Feldhoff, A., Lohaus, L., Haist, M., & Bigall, N. C. (2021). Influence of low-pressure treatment on the morphological and compositional stability of microscopic ettringite. Materials, 14(11), Artikel 2720. https://doi.org/10.3390/ma14112720
Ramadan, W., Feldhoff, A., & Bahnemann, D. (2021). Assessing the photocatalytic oxygen evolution reaction of BiFeO3 loaded with IrO2 nanoparticles as cocatalyst. Solar Energy Materials and Solar Cells, 232, Artikel 111349. https://doi.org/10.1016/j.solmat.2021.111349