Šepelák, V., Feldhoff, A., Heitjans, P., Krumeich, F., Menzel, D., Litterst, F. J., Bergmann, I., & Becker, K. D. (2006). Nonequilibrium cation distribution, canted spin arrangement, and enhanced magnetization in nanosized MgFe2O4 prepared by a one-step mechanochemical route. Chemistry of materials, 18(13), 3057-3067. https://doi.org/10.1021/cm0514894
Šepelák, V., Indris, S., Bergmann, I., Feldhoff, A., Becker, K. D., & Heitjans, P. (2006). Nonequilibrium cation distribution in nanocrystalline MgAl2O4 spinel studied by 27Al magic-angle spinning NMR. SOLID STATE IONICS, 177(26-32 SPEC. ISS.), 2487-2490. https://doi.org/10.1016/j.ssi.2006.04.014
Wessels, K., Feldhoff, A., Wark, M., Rathousky, J., & Oekermann, T. (2006). Low-temperature preparation of crystalline nanoporous TiO2 films by surfactant-assisted anodic electrodeposition. Electrochemical and Solid-State Letters, 9(6), C93-C96. https://doi.org/10.1149/1.2186430
Woltersdorf, J., Feldhoff, A., & Pippel, E. (2006). Interlayers in Metal Matrix Composites: Characterisation and Relevance for the Material Properties. In Metal Matrix Composites: Custom-made Materials for Automotive and Aerospace Engineering (S. 197-213). John Wiley and Sons Inc.. https://doi.org/10.1002/3527608117.ch8

2005


Feldhoff, A., Trichet, M. F., Mazerolles, L., & Backhaus-Ricoult, M. (2005). Electron microscopy study on the high-temperature oxidation of Si3N4-TiN ceramics: In situ and ex situ investigations. Journal of the European Ceramic Society, 25(10 SPEC. ISS.), 1733-1742. https://doi.org/10.1016/j.jeurceramsoc.2004.12.003
Mazerolles, L., Feldhoff, A., Trichet, M. F., & Backhaus-Ricoult, M. (2005). Oxidation behaviour of Si3N4-TiN ceramics under dry and humid air at high temperature. Journal of the European Ceramic Society, 25(10 SPEC. ISS.), 1743-1748. https://doi.org/10.1016/j.jeurceramsoc.2004.12.016
Šepelák, V., Bergmann, I., Feldhoff, A., Heitjans, P., Litterst, F. J., & Becker, K. D. (2005). Mechanosynthesis of spinel ferrite nanoparticles followed by Mössbauer spectroscopy. Hyperfine Interactions, 165(1-4), 81-87. https://doi.org/10.1007/s10751-006-9251-3
Wang, H., Tablet, C., Feldhoff, A., & Caro, J. (2005). A cobalt-free oxygen-permeable membrane based on the perovskite-type oxide Ba0.5Sr0.5Zn0.2Fe0.8O 3-δ. Advanced materials, 17(14), 1785-1788. https://doi.org/10.1002/adma.200401608
Wang, H., Tablet, C., Feldhoff, A., & Caro, J. (2005). Investigation of phase structure, sintering, and permeability of perovskite-type Ba0.5Sr0.5Co0.8Fe 0.2O3-δ membranes. Journal of membrane science, 262(1-2), 20-26. https://doi.org/10.1016/j.memsci.2005.03.046

2004


Klein, R., Desmaison-Brut, M., Medri, V., Feldhoff, A., & Desmaison, J. (2004). Mechanical properties of electroconductive ceramic composites produced by hot isostatic pressing. Key Engineering Materials, 264-268(II), 881-884. https://doi.org/10.4028/www.scientific.net/kem.264-268.881