Publikationen der AG Feldhoff

Zeige Ergebnisse 221 - 230 von 231

2003


Desmaison-Brut, M., Klein, R., Feldhoff, A., & Desmaison, J. (2003). High temperature oxidation behaviour of a hot isostatically pressed silicon nitride-titanium diboride ceramic composite. (High Temperature Corrosion and Materials Chemistry; Nr. IV). The Electrochemical Society.
Feldhoff, A., Trichet, M. F., Mazerolles, L., & Backhaus-Ricoult, M. (2003). High-temperature oxidation of Si3N4-TiN composites: Mechanisms and kinetics. (High Temperature Corrosion and Materials Chemistry; Nr. IV). The Electrochemical Society.

2000


Feldhoff, A., Pippel, E., & Woltersdorf, J. (2000). Interface engineering of carbon-fiber reinforced Mg-Al alloys. Advanced Engineering Materials, 2(8), 471-480. https://doi.org/10.1002/1527-2648(200008)2:8<471::AID-ADEM471>3.0.CO;2-S
Feldhoff, A., Pippel, E., & Woltersdorf, J. (2000). Tin coatings in C/Mg-Al composites: Microstructure, nanochemistry and function. Philosophical Magazine A: Physics of Condensed Matter, Structure, Defects and Mechanical Properties, 80(3), 659-672. https://doi.org/10.1080/01418610008212074
Woltersdorf, J., Feldhoff, A., & Lichtenberger, O. (2000). Complex bonding of titanium nitride layers in C/Mg composites revealed by ELNES features. Crystal research and technology, 35(6), 653-661. https://doi.org/10.1002/1521-4079(200007)35:6/7<653::AID-CRAT653>3.0.CO;2-N

1999


Feldhoff, A., Pippel, E., & Woltersdorf, J. (1999). Carbon-fibre reinforced magnesium alloys: Nanostructure and chemistry of interlayers and their effect on mechanical properties. Journal of microscopy, 196(2), 185-193. https://doi.org/10.1046/j.1365-2818.1999.00618.x
Feldhoff, A., Pippel, E., & Woltersdorf, J. (1999). Structure and composition of ternary carbides in carbon fibre reinforced Mg-Al alloys. Philosophical Magazine A: Physics of Condensed Matter, Structure, Defects and Mechanical Properties, 79(6), 1263-1277. https://doi.org/10.1080/01418619908210360

1998


Woltersdorf, J., Feldhoff, A., & Pippel, E. (1998). Formation, composition and effect of carbides in C-fibre reinforced Mg-Al alloys. Erzmetall: Journal for Exploration, Mining and Metallurgy, 51(9), 616-621.

1997


Feldhoff, A., Pippel, E., & Woltersdorf, J. (1997). Interface reactions and fracture behaviour of fibre-reinforced Mg/Al alloys. Journal of microscopy, 185(2), 122-131. https://doi.org/10.1046/j.1365-2818.1997.d01-611.x
Hähnel, A., Pippel, E., Feldhoff, A., Schneider, R., & Woltersdorf, J. (1997). Reaction layers in MMCs and CMCs: Structure, composition and mechanical properties. Materials Science and Engineering A, 237(2), 173-179. https://doi.org/10.1016/S0921-5093(97)00127-5